Availability: | |
---|---|
Quantity: | |
LJ
Product Description:
We can produce Steel sleeve for winding non-ferrous sheet and strip of various materials
and models according to customer needs.
Max length | 3000mm |
Max weight | 15000kg |
Application | Industrial Equipment and Mechinique Equipment |
Processing | Forging+machining+heating Treatment |
Design Support | Pro-E, UG,SolidWorks,AutoCad, PDF |
Heat treatment | N,N+T,Q+T or as customer's requirement |
Material:
carbon steel | 1010 20 35# 45# 16Mn S355J2 SA350 A105 A266 |
Alloy steel | 15CrMo 14Cr1Mo 20SiMn 18CrNiMo7-6 42CrMo4 34CrNiMo6 30CrNiMo8 4140 4340 F22 |
Mold steel | H11 H13 |
Heat-resistant steel | 1Cr13 2Cr13 F91 F92 X21CrMoV121 F6NM |
stainless steel | 304 321 316L 316LN 347 310 F51 F44 F55 F53 F60 15-5PH 17-4PH 1Cr17Ni2 |
Nickel-based alloys | 8810 8825 8120 GH4625 GH4169 GH4133 C276 |
Titanium alloy | TC4 TC6 TC11 |
1Cr11Ni2W2MoV has good comprehensive mechanical properties. It has been widely used in the air industry to make important components such as engine blades, disks, and shafts that work below 600 ° C.
Chemical Composition(%)
C | Si | Mn | S | P | Cr | Ni | V | Mo | W |
0.10~0.16 | ≤0.60 | ≤0.60 | ≤0.030 | ≤0.035 | 10.50~12.00 | 1.40~1.80 | 0.18~0.30 | 0.35~0.50 | 1.50~2.00 |
Heat Treatment and Mechanical Property
Qenching | Tempering | Tensile Strength σb (MPa) | Yield Strength σ0.2 (MPa) | Elongation δ5 (%) | Sectional shrinkage rate ψ (%) | Impact Akv (J) |
1000-1020℃ Oil-quenched | 540-600℃ Air-cooled | ≥1080 | ≥885 | ≥12 | ≥50 | ≥55 |
Product Description:
We can produce Steel sleeve for winding non-ferrous sheet and strip of various materials
and models according to customer needs.
Max length | 3000mm |
Max weight | 15000kg |
Application | Industrial Equipment and Mechinique Equipment |
Processing | Forging+machining+heating Treatment |
Design Support | Pro-E, UG,SolidWorks,AutoCad, PDF |
Heat treatment | N,N+T,Q+T or as customer's requirement |
Material:
carbon steel | 1010 20 35# 45# 16Mn S355J2 SA350 A105 A266 |
Alloy steel | 15CrMo 14Cr1Mo 20SiMn 18CrNiMo7-6 42CrMo4 34CrNiMo6 30CrNiMo8 4140 4340 F22 |
Mold steel | H11 H13 |
Heat-resistant steel | 1Cr13 2Cr13 F91 F92 X21CrMoV121 F6NM |
stainless steel | 304 321 316L 316LN 347 310 F51 F44 F55 F53 F60 15-5PH 17-4PH 1Cr17Ni2 |
Nickel-based alloys | 8810 8825 8120 GH4625 GH4169 GH4133 C276 |
Titanium alloy | TC4 TC6 TC11 |
1Cr11Ni2W2MoV has good comprehensive mechanical properties. It has been widely used in the air industry to make important components such as engine blades, disks, and shafts that work below 600 ° C.
Chemical Composition(%)
C | Si | Mn | S | P | Cr | Ni | V | Mo | W |
0.10~0.16 | ≤0.60 | ≤0.60 | ≤0.030 | ≤0.035 | 10.50~12.00 | 1.40~1.80 | 0.18~0.30 | 0.35~0.50 | 1.50~2.00 |
Heat Treatment and Mechanical Property
Qenching | Tempering | Tensile Strength σb (MPa) | Yield Strength σ0.2 (MPa) | Elongation δ5 (%) | Sectional shrinkage rate ψ (%) | Impact Akv (J) |
1000-1020℃ Oil-quenched | 540-600℃ Air-cooled | ≥1080 | ≥885 | ≥12 | ≥50 | ≥55 |